High temperature oxidation and corrosion of a porous Si2N2O-ZrO2 composite material:
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Buch |
Sprache: | English |
Veröffentlicht: |
1996
|
Schlagworte: | |
Beschreibung: | Göteborg, Univ., Diss., 1996 |
Beschreibung: | Getr. Zählung graph. Darst. |
ISBN: | 9171973524 |
Internformat
MARC
LEADER | 00000nam a2200000 c 4500 | ||
---|---|---|---|
001 | BV011385408 | ||
003 | DE-604 | ||
005 | 00000000000000.0 | ||
007 | t | ||
008 | 970616s1996 d||| m||| 00||| eng d | ||
020 | |a 9171973524 |9 91-7197-352-4 | ||
035 | |a (OCoLC)70192447 | ||
035 | |a (DE-599)BVBBV011385408 | ||
040 | |a DE-604 |b ger |e rakddb | ||
041 | 0 | |a eng | |
049 | |a DE-19 |a DE-355 |a DE-29T | ||
100 | 1 | |a Heim, Maiken |e Verfasser |4 aut | |
245 | 1 | 0 | |a High temperature oxidation and corrosion of a porous Si2N2O-ZrO2 composite material |c Maiken Heim |
264 | 1 | |c 1996 | |
300 | |a Getr. Zählung |b graph. Darst. | ||
336 | |b txt |2 rdacontent | ||
337 | |b n |2 rdamedia | ||
338 | |b nc |2 rdacarrier | ||
500 | |a Göteborg, Univ., Diss., 1996 | ||
650 | 0 | 7 | |a Hochtemperaturkorrosion |0 (DE-588)4132415-8 |2 gnd |9 rswk-swf |
650 | 0 | 7 | |a Zirkoniumoxidkeramik |0 (DE-588)4280132-1 |2 gnd |9 rswk-swf |
655 | 7 | |0 (DE-588)4113937-9 |a Hochschulschrift |2 gnd-content | |
655 | 7 | |a Siliciumoxynitride |2 gnd |9 rswk-swf | |
689 | 0 | 0 | |a Siliciumoxynitride |A f |
689 | 0 | 1 | |a Zirkoniumoxidkeramik |0 (DE-588)4280132-1 |D s |
689 | 0 | 2 | |a Hochtemperaturkorrosion |0 (DE-588)4132415-8 |D s |
689 | 0 | |5 DE-604 | |
999 | |a oai:aleph.bib-bvb.de:BVB01-007652237 |
Datensatz im Suchindex
_version_ | 1804125896827731968 |
---|---|
any_adam_object | |
author | Heim, Maiken |
author_facet | Heim, Maiken |
author_role | aut |
author_sort | Heim, Maiken |
author_variant | m h mh |
building | Verbundindex |
bvnumber | BV011385408 |
ctrlnum | (OCoLC)70192447 (DE-599)BVBBV011385408 |
format | Book |
fullrecord | <?xml version="1.0" encoding="UTF-8"?><collection xmlns="http://www.loc.gov/MARC21/slim"><record><leader>01229nam a2200361 c 4500</leader><controlfield tag="001">BV011385408</controlfield><controlfield tag="003">DE-604</controlfield><controlfield tag="005">00000000000000.0</controlfield><controlfield tag="007">t</controlfield><controlfield tag="008">970616s1996 d||| m||| 00||| eng d</controlfield><datafield tag="020" ind1=" " ind2=" "><subfield code="a">9171973524</subfield><subfield code="9">91-7197-352-4</subfield></datafield><datafield tag="035" ind1=" " ind2=" "><subfield code="a">(OCoLC)70192447</subfield></datafield><datafield tag="035" ind1=" " ind2=" "><subfield code="a">(DE-599)BVBBV011385408</subfield></datafield><datafield tag="040" ind1=" " ind2=" "><subfield code="a">DE-604</subfield><subfield code="b">ger</subfield><subfield code="e">rakddb</subfield></datafield><datafield tag="041" ind1="0" ind2=" "><subfield code="a">eng</subfield></datafield><datafield tag="049" ind1=" " ind2=" "><subfield code="a">DE-19</subfield><subfield code="a">DE-355</subfield><subfield code="a">DE-29T</subfield></datafield><datafield tag="100" ind1="1" ind2=" "><subfield code="a">Heim, Maiken</subfield><subfield code="e">Verfasser</subfield><subfield code="4">aut</subfield></datafield><datafield tag="245" ind1="1" ind2="0"><subfield code="a">High temperature oxidation and corrosion of a porous Si2N2O-ZrO2 composite material</subfield><subfield code="c">Maiken Heim</subfield></datafield><datafield tag="264" ind1=" " ind2="1"><subfield code="c">1996</subfield></datafield><datafield tag="300" ind1=" " ind2=" "><subfield code="a">Getr. Zählung</subfield><subfield code="b">graph. Darst.</subfield></datafield><datafield tag="336" ind1=" " ind2=" "><subfield code="b">txt</subfield><subfield code="2">rdacontent</subfield></datafield><datafield tag="337" ind1=" " ind2=" "><subfield code="b">n</subfield><subfield code="2">rdamedia</subfield></datafield><datafield tag="338" ind1=" " ind2=" "><subfield code="b">nc</subfield><subfield code="2">rdacarrier</subfield></datafield><datafield tag="500" ind1=" " ind2=" "><subfield code="a">Göteborg, Univ., Diss., 1996</subfield></datafield><datafield tag="650" ind1="0" ind2="7"><subfield code="a">Hochtemperaturkorrosion</subfield><subfield code="0">(DE-588)4132415-8</subfield><subfield code="2">gnd</subfield><subfield code="9">rswk-swf</subfield></datafield><datafield tag="650" ind1="0" ind2="7"><subfield code="a">Zirkoniumoxidkeramik</subfield><subfield code="0">(DE-588)4280132-1</subfield><subfield code="2">gnd</subfield><subfield code="9">rswk-swf</subfield></datafield><datafield tag="655" ind1=" " ind2="7"><subfield code="0">(DE-588)4113937-9</subfield><subfield code="a">Hochschulschrift</subfield><subfield code="2">gnd-content</subfield></datafield><datafield tag="655" ind1=" " ind2="7"><subfield code="a">Siliciumoxynitride</subfield><subfield code="2">gnd</subfield><subfield code="9">rswk-swf</subfield></datafield><datafield tag="689" ind1="0" ind2="0"><subfield code="a">Siliciumoxynitride</subfield><subfield code="A">f</subfield></datafield><datafield tag="689" ind1="0" ind2="1"><subfield code="a">Zirkoniumoxidkeramik</subfield><subfield code="0">(DE-588)4280132-1</subfield><subfield code="D">s</subfield></datafield><datafield tag="689" ind1="0" ind2="2"><subfield code="a">Hochtemperaturkorrosion</subfield><subfield code="0">(DE-588)4132415-8</subfield><subfield code="D">s</subfield></datafield><datafield tag="689" ind1="0" ind2=" "><subfield code="5">DE-604</subfield></datafield><datafield tag="999" ind1=" " ind2=" "><subfield code="a">oai:aleph.bib-bvb.de:BVB01-007652237</subfield></datafield></record></collection> |
genre | (DE-588)4113937-9 Hochschulschrift gnd-content Siliciumoxynitride gnd |
genre_facet | Hochschulschrift Siliciumoxynitride |
id | DE-604.BV011385408 |
illustrated | Illustrated |
indexdate | 2024-07-09T18:08:51Z |
institution | BVB |
isbn | 9171973524 |
language | English |
oai_aleph_id | oai:aleph.bib-bvb.de:BVB01-007652237 |
oclc_num | 70192447 |
open_access_boolean | |
owner | DE-19 DE-BY-UBM DE-355 DE-BY-UBR DE-29T |
owner_facet | DE-19 DE-BY-UBM DE-355 DE-BY-UBR DE-29T |
physical | Getr. Zählung graph. Darst. |
publishDate | 1996 |
publishDateSearch | 1996 |
publishDateSort | 1996 |
record_format | marc |
spelling | Heim, Maiken Verfasser aut High temperature oxidation and corrosion of a porous Si2N2O-ZrO2 composite material Maiken Heim 1996 Getr. Zählung graph. Darst. txt rdacontent n rdamedia nc rdacarrier Göteborg, Univ., Diss., 1996 Hochtemperaturkorrosion (DE-588)4132415-8 gnd rswk-swf Zirkoniumoxidkeramik (DE-588)4280132-1 gnd rswk-swf (DE-588)4113937-9 Hochschulschrift gnd-content Siliciumoxynitride gnd rswk-swf Siliciumoxynitride f Zirkoniumoxidkeramik (DE-588)4280132-1 s Hochtemperaturkorrosion (DE-588)4132415-8 s DE-604 |
spellingShingle | Heim, Maiken High temperature oxidation and corrosion of a porous Si2N2O-ZrO2 composite material Hochtemperaturkorrosion (DE-588)4132415-8 gnd Zirkoniumoxidkeramik (DE-588)4280132-1 gnd |
subject_GND | (DE-588)4132415-8 (DE-588)4280132-1 (DE-588)4113937-9 |
title | High temperature oxidation and corrosion of a porous Si2N2O-ZrO2 composite material |
title_auth | High temperature oxidation and corrosion of a porous Si2N2O-ZrO2 composite material |
title_exact_search | High temperature oxidation and corrosion of a porous Si2N2O-ZrO2 composite material |
title_full | High temperature oxidation and corrosion of a porous Si2N2O-ZrO2 composite material Maiken Heim |
title_fullStr | High temperature oxidation and corrosion of a porous Si2N2O-ZrO2 composite material Maiken Heim |
title_full_unstemmed | High temperature oxidation and corrosion of a porous Si2N2O-ZrO2 composite material Maiken Heim |
title_short | High temperature oxidation and corrosion of a porous Si2N2O-ZrO2 composite material |
title_sort | high temperature oxidation and corrosion of a porous si2n2o zro2 composite material |
topic | Hochtemperaturkorrosion (DE-588)4132415-8 gnd Zirkoniumoxidkeramik (DE-588)4280132-1 gnd |
topic_facet | Hochtemperaturkorrosion Zirkoniumoxidkeramik Hochschulschrift Siliciumoxynitride |
work_keys_str_mv | AT heimmaiken hightemperatureoxidationandcorrosionofaporoussi2n2ozro2compositematerial |